water toughening

水冷韧化处理

  • After water toughening the superhigh manganese steel was tempered at various temperatures and then treated cryogenically at-196 ℃ .

    其工艺过程是: 处理后,在不同温度回火处理,然后马上在-196℃下深冷处理。

  • Large scale high manganese steel alligator board produced by EPC process can meet the request of design and use with hot remained water toughening treatment .

    消失模铸造生产大型高锰钢颚板,并按设计的工艺要求进行生产,利用余热 处理。

  • The method of producing the teeth of bin in power shovel by vanishing mould casting and the method of operation of water toughening were presented .

    介绍了用消失模铸造生产电铲斗齿的工艺方法以及 处理的操作要点。

  • The effects of water toughening quality on the toughness at low temperature of high-manganese steel was studied using impact - tests .

    通过冲击试验,研究了 处理质量对高锰钢低温韧性的影响。

  • Special compound for automobile water tank cover was prepared with PP as matrix resin talc powder and POE as reinforcing agent and toughening agent respectively the effects of talc and POE on the property of the compound were studied .

    以聚丙烯为基体树脂,活化滑石粉为增强剂,POE为 增韧剂,研制出了汽车 水箱面罩专用料。

  • Hot Remained Water Toughening Treatment for Large Scale Alligator Board in EPC Processing

    消失模铸造大型高锰钢颚板的余热 处理

  • The effect of water toughening treatment on structure and properties of high manganese steel with trace Cr V Mo is studied in the present research .

    研究了 处理工艺对Cr、V、Mo合金高锰钢金相组织和力学性能的影响。

  • Study of Water Toughening Treatment Process of High Manganese Wear-resistant Steel Castings with Residual Heat

    高锰钢耐磨铸件铸态余热 处理工艺研究

  • Effect of water toughening temperature on microstructure and properties of super-high manganese steel with trace boron

    处理温度对含硼超高锰钢组织和性能的影响

  • Direct Water Toughening Process for High Mn Steel

    高锰钢铸件的直接 处理工艺

  • In other words when the water toughening process is applied the operation temperature is not high enough which causes some carbine is kept rather than dissolved and uniform Austenite is not obtained .

    处理时加热温度不够高,未能把碳化物溶解,而使其保留了下来,未得到均匀的奥氏体组织。